Following test is also known as microhardness test
Knoop hardness test
Hardness testing is a common method used to determine a material's resistance to permanent deformation, such as indentation. Different tests use various indenter shapes, loads, and procedures, making them suitable for different materials and applications.
Microhardness testing is a specific category of hardness tests where very low loads (typically less than 1 kgf) are applied, and the resulting indentation is very small. This makes them ideal for testing:
Let's look at the hardness tests listed in the options:
Brinell Hardness Test: This test uses a hardened steel or carbide ball indenter and relatively high loads (typically 500 to 3000 kgf). The indentation is relatively large, making it suitable for testing bulk materials, especially those with coarse grain structures. It is generally considered a macrohardness test.
The Brinell hardness number ($\text{HBW}$) is calculated using the formula:
$\text{HBW} = \frac{2P}{\pi D(D - \sqrt{D^2 - d^2})}$
where $P$ is the applied load, $D$ is the indenter diameter, and $d$ is the indentation diameter.
Vickers Hardness Test: This test uses a square-based diamond pyramid indenter. It is versatile and can be used for both macro and microhardness testing depending on the applied load. Loads can range from very low (a few grams) to high (100 kgf or more). When very low loads are used, it is considered a microhardness test.
The Vickers hardness number ($\text{HV}$) is calculated using the formula:
$\text{HV} = \frac{2P \sin(136^\circ/2)}{d^2} = \frac{1.854 P}{d^2}$
where $P$ is the applied load and $d$ is the average length of the two diagonals of the indentation.
Rockwell Hardness Test: This test measures hardness based on the depth of penetration of the indenter under specific loads. It uses different indenters (diamond cone or steel ball) and various load combinations, resulting in different Rockwell scales (e.g., HRC, HRB). It is primarily a macrohardness test, though superficial Rockwell scales use lighter loads. It does not typically fall under the microhardness category in the same way as low-load Vickers or Knoop.
The Rockwell hardness number is read directly from the testing machine, based on the difference between the minor and major load penetration depths.
Knoop Hardness Test: This test also uses a diamond pyramid indenter, but it has a rhombic base shape with different angles (172.5 degrees and 130 degrees) leading to an elongated indentation. This test is specifically designed for microhardness testing, typically using very low loads (from a few grams to 1 kgf). The elongated indentation is particularly useful for testing brittle materials or areas with steep hardness gradients, as it causes less cracking than a square indentation.
The Knoop hardness number ($\text{HK}$) is calculated using the formula:
$\text{HK} = \frac{P}{A_p} = \frac{P}{0.07028 l^2}$
where $P$ is the applied load, $A_p$ is the projected area of the indentation, and $l$ is the length of the long diagonal of the indentation.
Based on the characteristics of these tests, the Knoop hardness test is primarily known and used specifically as a microhardness test due to its design and typical load ranges.
The fundamental property of material able to resist abrasion is called as
Yielding is defined as the transition from _________ to ____________.
___________ is the collective term for the physical manifestations of the defects like cracks, spalling, pop out, staining and corrosion.